On the final leg of sandblasting, I removed the torsion bars and spring plates to get a thorough sandblast and rust-proof in-between. In order to do this, I made the pan level, knocked the spring plates out just enough to pop off of their stops and measured the angle with an angle finder so that I could reinstall them correctly. 16 degrees on both sides!
With these removed, I finished sandblasting the pan. I underestimated how much of a hassle sandblasting this pan myself would be. It took me around two months doing it myself in my free time. If I were to do it again, I would just drop it off somewhere. Anyway, I ended up doing it in sections, making the realization that I couldn't do the whole thing at one time with the small sandblaster that I had. I carefully rust-proofed it as I went with phosphoric acid.
It's finally completed and rust free. there were several areas where some stubborn undercoating had to be removed by hand, but it wasn't too bad.
| Final Cleanup Before Paint |
👍